Why does nobody talk about torque-to-yield bolts stretching on the first reuse | Auto Mechanics - Freelance Forum - The Community for Independent Professionals
Why does nobody talk about torque-to-yield bolts stretching on the first reuse
I always figured you could get away with head bolts twice if they looked clean, but last month I actually measured a set off a 2.4 in my garage and the numbers bugged me. Stock length was right at 4.37 inches and two of them came out at 4.42, which is past the spec I dug up in a forum thread from a guy down in Waco. Turns out those factory torque-to-yield bolts are designed to stretch once and relax, so reusing them is like putting a used rubber band back on. I put a caliper on every bolt I pull now, takes about ten extra minutes and it settled my mind. The part that got me was how the bolt still torqued fine and felt good, no warning at all before it would have let go. Curious if you all keep a spec sheet handy for stretch limits or just swap them out on principle.
Ran into the same thing on a 5.3 a couple years back and it weirded me out. Pulled the bolts, they all looked perfect, threads clean, heads not chewed up, so I ran them again and it ran fine for about a year. Then a buddy talked me into actually checking the lengths against spec and half of them were over the limit, which freaked me out enough that I tore it back down and put new ones in. The scary part is exactly what you said, they torque up and feel solid so you get no sign at all that they are done. I keep a printout of the specs in my toolbox now and check every set I pull, cheap insurance for ten minutes of work.